Lattice Defects in Hydrogenated and HPT Processed Pd
- Author(s)
- Daria Setman, Maciej Krystian, Michael Zehetbauer
- Abstract
Pure palladium (99.95%) was hydrogenated, subsequently deformed by High Pressure Torsion (HPT) and analyzed by differential scanning calorimetry (DSC). For comparison some hydrogen-free HPT processed samples were also investigated. In case of the hydrogenated HPT Pd, the concentration of single / double vacancies is noticeably higher. The importance of hydrogen for the formation and stabilization of vacancy type defects and dislocations is discussed.
- Organisation(s)
- Physics of Nanostructured Materials
- External organisation(s)
- Austrian Research Centers GmbH (ARC Seibersdorf)
- Journal
- Materials Science Forum
- Volume
- 584-586
- Pages
- 355-360
- No. of pages
- 6
- ISSN
- 0255-5476
- DOI
- https://doi.org/10.4028/www.scientific.net/MSF.584-586.355
- Publication date
- 2008
- Peer reviewed
- Yes
- Austrian Fields of Science 2012
- 103023 Polymer physics, 210006 Nanotechnology, 103018 Materials physics
- Portal url
- https://ucrisportal.univie.ac.at/en/publications/e0c07461-b401-4a81-905f-7016df73e489